Boronizing of Ti-6Al-4V Eli by powder pack method for biomedical application

Document Type

Conference Proceeding

Publication Date

1-1-2005

Abstract

The boronization of Ti-6Al-4V Eli alloy was prepared by powder pack method. As a result of the boronizing process, the boride coating was presented as titanium boride (TiB) with a coating thickness about 2-9 μm. Furthermore, the microhardness of the boron coating was about 500-800 HK. The microstructure of the coating was also observed by the optical microscope. ©2005 IEEE.

Identifier

28444463205 (Scopus)

Publication Title

Proceedings of the IEEE Annual Northeast Bioengineering Conference Nebec

ISSN

1071121X

First Page

193

Last Page

194